jmlchart08

Fig. 8 – Fire the Shell Mould

STEP 8:
The tree is fired at a high temperature to sinter the ceramics which make up the mold to give it significant strength, and this process also preheats the mold for pouring, so that the thermal shock of the molten metal entering the shell on the subsequent pouring operation will not break the thin ceramic wall.